Slump Test of Concrete

Image
searchfeed Slump tEST (IS:1199-1959) OBJECTIVe To determine the workability or consistency of concrete mix of given proportion by slump test.   REFERENCE STANDARDS IS : 1199-1959 – Methods of tests for Slump of concrete. EQUIPMENT & APPARATUS §   Slump Cone with base plate §   Tampering Rod PROCEDURE  Take the sample concrete from the discharge location. The internal surface of the slump cone is to be thoroughly cleaned and placed on a smooth, horizontal, rigid and non absorbent surface. Place the mixed concrete in the cleaned slump cone in 4 layers each approximately 1/4 in height of the mould. Tamp each layer 25 times with tamping rod. Remove the cone immediately, rising it slowly and carefully in the vertical direction. As soon as the concrete settlement comes to a stop, measure the subsistence of the concrete in cms, which gives the slump. searchfeed SAFETY & PRECAUTIONS The strokes are

ACCELERATED CURING TEST OF CONCRETE (IS:9013-1978)

Image
ACCELERATED CURING TEST OF CONCRETE (IS:9013-1978) OBJECTIVE Normally, the strength of concrete is found out after 7 days and 28 days. For some construction activities, it may be too late and need to know the strength earlier.   REFERENCE STANDARDS IS: 9013-1978-Method of making, curing and determining compressive strength of accelerated cured concrete test specimen. EQUIPMENT & APPARATUS §   Accelerated curing tank §   Compression Testing                                                                                                Accelerated Curing Tank PROCEDURE 1.                    Prepare the concrete cube specimen and store it in moist air of at least 90% relative humidity and at a temperature of 27+2 o C for 23 hrs + 15 minutes. 2.                  Lower the specimen, into a curing tank with water at 100   0 C and keep it totally immersed for 3 ½ hours + 5 minutes 3.                  The temperature of water shall not drop more than 3oC after

EXTERNAL PAINTING ON BUILDING

Image
METHOD STATEMENT FOR EXTERNAL PAINTING          INTRODUCTION:   The purpose of this Method Statement for Painting of Building is to describe in detail the procedure to be adopted.           OBJECT: Approved Ele vation drawings with color scheme MATERIALS : Paint and Finishing Materials : It should be as per approved color and code number.   Putty & Primer : - It should be as per approved make . EQUIPMENT AND TOOLS: Air compressor, Spray Gun, Jhoola/Suspended platform, Fiber Blade, Paint Brush (as per required size), Painting roller, Masking tape, Sand paper, Polythene sheet, old cloth     HEALTH AND SAFETY PROVISIONS: a)   Inspect to ensure that safety belt, safety goggle and safety mask has been used before start of work to avoid any accident. b)   Inspect and ensure that all ropes & hanging platform are safe for work. c)    Ensure that one helper should be available at terrace level during painting work to check all the knots of ropes are p

Tools for Masson using in Tile Fixing

Image
                        Tools for Masson using in Tile Fixing Sprit level 600mm long, Coconut Broom, Measuring Tape, Hand Tile Cutting Machine, Rubber Hammer, Scraper, Tile cleaning machine , Grooving trowel, soft brush. MATERIAL Ceramic Tiles, Vitrified Tile, Cement, Sand, PVC Spacers, PVC Corners ,sponge, water, grouting material , floor cleaning liquid

How to fix the Tile on Wall & Floor

Image
searchfeed                          How to fix the Tile on Wall & Floor 1.    First of all chipping should be done on all RCC members so as to remove any extra concrete/ cement mortar on the surface. 2.    Level should be marked on the walls with Mason thread 3.    Tile start point & Layout shall be done according to the GFC drawing. 4.    Tile should be soaked in water i.e. vitrified tile as per manufacturer recommendation and ceramic tile for 2-3 hours. 5.    Base concrete or the RCC slab on which the tiles are to be laid shall be cleaned and wetted with water and thereafter cement slurry are to be spread over the surface. 6.    Level tip are to be established 7.    The bedding for the tile shall be with cement mortar 1:41 cement: 4 stone dust).   The average thickness of the bedding shall be 20-30 mm for flooring & 15-20mm (in 2 layers) for dado 8.    Cement mortar are to be spread up to maximum of 150 Sft of floor area at one go. The laid mortar

How to construct Storm/Rain Water Drainage system

Image
searchfeed HOW TO CONSTRUCT STORM WATER SYSTEM                                                  INTRODUCTION A storm water system is a system to manage runoff from rainfall and maintain the underground water table. OBJECTIVE: Main objective of this method statement is to complete the work in a uniform way across all projects with accuracy and efficiency.   MATERIAL Bricks, Coarse Sand, Cement, Aggregate, RCC Covers, Reinforcement steel, PVC slotted pipe, Gravels, MS Rungs, MS Grating etc.   APPARATUS / EQUIPMENT JCB / Excavator, Tractor with Trolley/Tippers, Plate Compactor, Double Drum Roller, Mixture Machine, Auto Level, Mason Thread, Rope, Measuring tape, Plumb bob, karni, Basuli, Boring machine, Water tanker.   HEALTH AND SAFETY PROVISION ·          Permission from the engineer in charge shall be taken before any excavation commences, and all persons involved in the task shall be fully briefed. ·          Fencing and safety signage to